Simulating convection and macrosegregation in superalloys

  • S. D. Felicelli
  • , D. R. Poirier
  • , A. F. Giamei
  • , J. C. Heinrich

Research output: Contribution to journal › Article › peer-review

Abstract

Numerical simulations using a mathematical model of the dendritic solidification of multicomponent alloys that includes thermosolutal convection and macrosegregation were conducted on nickel-based alloys. The results show that segregation patterns vary greatly with cooling conditions, adopting several shapes and levels of intensity. In addition, the segregation patterns are particularly sensitive to the values of the equilibrium partition coefficients of the alloy components.

Original languageEnglish (US)
Pages (from-to)21-25
Number of pages5
JournalJOM
Volume49
Issue number3
DOIs
StatePublished - Mar 1997

ASJC Scopus subject areas

  • General Materials Science
  • General Engineering

Fingerprint

Dive into the research topics of 'Simulating convection and macrosegregation in superalloys'. Together they form a unique fingerprint.

Cite this